All MetalShaping

Go Back   All MetalShaping > Search Forums
  Today's Posts Posts for Last 7 Days Posts for Last 14 Days  

Showing results 1 to 3 of 3
Search took 0.00 seconds.
Search: Posts Made By: crystallographic
Forum: Basic questions and answers 10-11-2018, 10:33 PM
Replies: 12
Views: 4,976
Posted By crystallographic
Yep. Yas, and .... yabetcha.

Yep.


Yas, and .... yabetcha.
Forum: Basic questions and answers 10-11-2018, 12:26 PM
Replies: 12
Views: 4,976
Posted By crystallographic
annealing metal alloys - 6061, done in the field

"Annealing" is a procedure done to soften metals with correct heating to correct temperatures, holding for a correct amount of time, and quenching at a given rate.

Different metal alloys require...
Forum: Basic questions and answers 10-10-2018, 09:18 PM
Replies: 12
Views: 4,976
Posted By crystallographic
Hi Wes, 6061 is not that bad once you get used...

Hi Wes,
6061 is not that bad once you get used to it, actually.
Yes, you can soften it a bit for 12-18 hours by heating to 650F - black marker burns off - then quench with cold water.