Default Starting with aluminum

Hey guys I've been playing around with steel forming 16g and got a big sheet of 16g 6061 from work. Now I have a few questions because I don't have a torch set up.

Is annealing necessary or is it just to make the workability Easier or am I running the risk of work hardening the material to the point of failure.

Also on the topic of annealing I've seen most people use 3000 series aluminum for working with how's 6061 compare as a product for doing forming? I have great ease of access to 6061 that's why I ask.
__________________
Wes
Reply With Quote
 

Thread Tools Search this Thread
Search this Thread:

Advanced Search
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is On

Forum Jump

All times are GMT -5. The time now is 12:19 PM.

Powered by vBulletin® Version 3.8.11
Copyright ©2000 - 2024, vBulletin Solutions Inc.