Default How to form 'X' bead?

How would you make this 'X' in the gastank endcap?
132.jpg

Thanks, Oj
__________________
oj higgins
Reply With Quote
  #2  
Old 07-20-2020, 09:13 AM
billfunk29 billfunk29 is offline
Member
 
Join Date: Oct 2013
Location: Minnesota
Posts: 319
Default X

I would use a router or chisel to cut the grooves in a wooden hammer form. Then pound it in with a rounded punch. You could also form the perimeter flange on the same hammer form. One of many ways.
__________________
Bill Funk
Reply With Quote
  #3  
Old 07-20-2020, 09:23 AM
crystallographic crystallographic is offline
MetalShaper of the Month October '14 , April '16, July 2020, Jan 2023
 
Join Date: Dec 2010
Location: Western Sierra Nevadas, Badger Hill, CA
Posts: 4,388
Default

Quote:
Originally Posted by ojh View Post
How would you make this 'X' in the gastank endcap?
Attachment 56874

Thanks, Oj

X-beads take some effort, very unlike using a leaf brake to criss-cross bend a tailgate panel.


Guessing yer metal is terne plate? (lead-coated steel)
These tank ends were likely press-formed using nice male-female steel dies.

Getting some round bar to match yer profile, cutting to fit and laying the three pcs in the gullets and tacking one side, flipping and welding, flipping again and welding, then smacking back to straight end level fit - gets you the male X "die" which is then skip welded onto some 1/4" plate.

Then you can rig the "Pullmax" nibbler for an upper die to close down over your terne material +X die combined - and a lower die to support/guide the plate. Then stroke that enough times to draw fully down over your X die.


Or set up to flow form the panel down over the X die, on the workbenchbench.


Or, cast up a lead/epoxy female die in a steel bolster (need both ends for that tank?) and then use about 15 tons to smoosh your panels.... 22ga DDQ or EDQ will work for end panels on that size suitcase.


Or machine some brass round bars to lay accurately on a blank surface, rivet then on and solder all around to simulate the artwork.


That catfish can be skinned in different ways.
__________________
Kent

http://www.tinmantech.com

"All it takes is a little practical experience to blow the he!! out of a perfectly good theory." --- Lloyd Rosenquist, charter member AWS, 1919.
Reply With Quote
  #4  
Old 07-20-2020, 11:49 AM
ojh ojh is offline
Member
 
Join Date: Nov 2009
Location: Shenandoah Valley, VA
Posts: 674
Default

I tried the form flow, considered getting different tooling from Kent to see if I get better results. It took forever to get 1 panel made and it wasn't finished. I've made an upper die for the Trumpf and trying to figure how to clamp and align it all together to do it in a machine.
134.jpg
I'd like to do 3 sets of them.
__________________
oj higgins
Reply With Quote
  #5  
Old 07-20-2020, 01:01 PM
crystallographic crystallographic is offline
MetalShaper of the Month October '14 , April '16, July 2020, Jan 2023
 
Join Date: Dec 2010
Location: Western Sierra Nevadas, Badger Hill, CA
Posts: 4,388
Default

Quote:
Originally Posted by ojh View Post
I tried the form flow, considered getting different tooling from Kent to see if I get better results. It took forever to get 1 panel made and it wasn't finished. I've made an upper die for the Trumpf and trying to figure how to clamp and align it all together to do it in a machine.
Attachment 56875
I'd like to do 3 sets of them.

OJ,
Just add the top layer with the X opening, clamp tight and chase the bead down with the rivet gun.
__________________
Kent

http://www.tinmantech.com

"All it takes is a little practical experience to blow the he!! out of a perfectly good theory." --- Lloyd Rosenquist, charter member AWS, 1919.
Reply With Quote
  #6  
Old 07-20-2020, 02:00 PM
ojh ojh is offline
Member
 
Join Date: Nov 2009
Location: Shenandoah Valley, VA
Posts: 674
Default

Quote:
Originally Posted by crystallographic View Post
OJ,
Just add the top layer with the X opening, clamp tight and chase the bead down with the rivet gun.
Tried it like that, didn't have 'top layer', I had C clamped the perimeter and 11ga strapping between clamps and form, they weren't very close to the X opening. I was wondering if the metal was too much area to stretch from and it needed clamping right at the edge of the X opening.
__________________
oj higgins
Reply With Quote
  #7  
Old 07-20-2020, 05:08 PM
crystallographic crystallographic is offline
MetalShaper of the Month October '14 , April '16, July 2020, Jan 2023
 
Join Date: Dec 2010
Location: Western Sierra Nevadas, Badger Hill, CA
Posts: 4,388
Default

Quote:
Originally Posted by ojh View Post
Tried it like that, didn't have 'top layer', I had C clamped the perimeter and 11ga strapping between clamps and form, they weren't very close to the X opening. I was wondering if the metal was too much area to stretch from and it needed clamping right at the edge of the X opening.

OJ,
"Close to halfway" ain't enuf for a serious grade on this metal whacking method.
Seriously, Bub....



Bite the $%@##&* bullet ... !

Make the top half, Clamp/BOLT it TIGHT, and bonk in the bead. (bolting is much less clamp-slippy when rattling in these beads )

You can do this - Times Six Each, for 3 sets - If you maintain the rigors.


If you need a better schnooble - let me know the bead radius ... and if you have a spare rivet set on hand to modify ... ?
__________________
Kent

http://www.tinmantech.com

"All it takes is a little practical experience to blow the he!! out of a perfectly good theory." --- Lloyd Rosenquist, charter member AWS, 1919.
Reply With Quote
  #8  
Old 07-21-2020, 08:38 AM
ojh ojh is offline
Member
 
Join Date: Nov 2009
Location: Shenandoah Valley, VA
Posts: 674
Default

Groan...
I guess I knew and just needed the telling.
Where do you get this 'terne'? I was going to do a heavy coat of ospho.
__________________
oj higgins
Reply With Quote
  #9  
Old 07-21-2020, 09:50 AM
Chris_Hamilton Chris_Hamilton is offline
Member
 
Join Date: Jan 2013
Location: Southisde Virginia
Posts: 329
Default

Terne is the material. Lead plated steel sheet.
__________________
Chris (trying to be the best me I can be)
Reply With Quote
  #10  
Old 07-21-2020, 12:53 PM
crystallographic crystallographic is offline
MetalShaper of the Month October '14 , April '16, July 2020, Jan 2023
 
Join Date: Dec 2010
Location: Western Sierra Nevadas, Badger Hill, CA
Posts: 4,388
Default

Quote:
Originally Posted by Chris_Hamilton View Post
Terne is the material. Lead plated steel sheet.

Righty-o, Chris ...


But the stuff is near-impossible to locate these past years.
I had to make a replacement 1914 roadster tank using my own supply of terne several years ago. Now I'd probably have to make repro tanks from Gal-X-C and that is darn sensitive to soldering heats - get it right or face the Black Patch of "lost time" scrubbing and tinning it back to bright ...!


Ron Naida probably has the best idea - make terne yourself - and he made a post here on his whole process of solder-coating enough sheet for a tank he built - as original.

A Primo Post !!!
__________________
Kent

http://www.tinmantech.com

"All it takes is a little practical experience to blow the he!! out of a perfectly good theory." --- Lloyd Rosenquist, charter member AWS, 1919.
Reply With Quote
Reply

Thread Tools Search this Thread
Search this Thread:

Advanced Search
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is On

Forum Jump

All times are GMT -5. The time now is 06:15 AM.

Powered by vBulletin® Version 3.8.11
Copyright ©2000 - 2024, vBulletin Solutions Inc.