Conventional hand hammers have had the striking heads made from a variety of materials for many long decades:
Hardened steel
Soft steel
Malleable iron
Tin
Brass
Lead
Copper
Aluminum
Bronze
Leather
Rubber
Plastic
Nylon
Urethane
Fiber
Wood
and other materials ...
Some of these hammer materials are used for "non-marking" and others are used for "non-sparking."

For metal shaping/planishing purposes, steel, rubber, leather, and various urethanes and polymers can find good application. Steel is the most common die material for hammering metal.
Vulcanized rubber and leather have been good elastic "soft" materials for hammering steel and aluminum sheet. Rubber compounds vary, as we see in the tire industry.
When I started vulcanizing rubber hammer heads for my Air Hammer in 1994 they worked pretty well, though I soon learned that urethanes could also be molded to these shapes and they could also be selected from a range of durometers/hardnesses.
From that point on I found that urethanes could also be compounded for a variety of applications - like suspension bushings in NASCAR chassis, for instance. So getting the durometer right is a good basic starting point.

For my own "velocity/impact" shrinking method that I developed specific dies for in my Air Hammer in 1994, I chose a hard polymer that is softer than hard steel, but holds up well when shrinking soft metals like some aluminum alloys, copper, and soft brass. This black polymer has worked well enough for us that it has seen no changes since 1994. We even used it in our Pullmax thumbnail dies, starting in 1995, using them also to shrink 20ga mild steel.

Since that early start I have experimented with a variety of urethane compounds from a variety of companies that have patents on their urethanes.

One that we offer for stretching aluminum does rapid reverse shaping on .040 3003 half hard, and sometimes with zero annealing.
P1030887 c.jpg
Waco gear leg fairings. Front pair have been shaped and then planished with our hard polymer non-rotating reverse dies.... below. Rear fairing is only roughed with the "Expansive" urethane hammer.
P1030922 c.jpg

This heat shied/air deflector was stretched using our urethane "Expansive" upper hammer over a shaped steel die.
P1030895 c.jpg
.063 3003 half hard, perforated aluminum

P1030899 c.jpg
Same part being reversed with the Expansive urethane hammer over a shaped steel die.

P1030900 c.jpg
Same part being shrunk with our Shrinking Set for Soft Metals - black hard polymer (softer than steel)

P1030904 c.jpg
.040 perf. aluminum, 3003 half hard, being stretched with the Oversized Roughing Head (3" dia. leather hammer) over a domed steel die.

P1030910 c.jpg
Showing finished/untrimmed anodized costume visors with unfinished bare visor. These parts' edges also shrunk with the Soft Metal Shrinking set.

P1030912 c.jpg
Art lamp part, .080 6061 "0" temper, with part annealed only after first round of heavy stretching with leather Oversized Roughing Head w/ domed steel lower die. Shrinking on edges done with the Shrinking Set for Soft Metals. After continued working, the metal develops a lot of stress, so the choice is to either anneal and then continue, or continue and then weld.

In summation, many of us prefer soft dies for stretching and shrinking because of the minimal surface marking and because of the smooth contours left for subsequent planishing operations. In some cases, an aggressive soft die can stretch very rapidly - without damaging the material, like the Waco fairings were done. I developed this method back when I was doing the Hughes H1 (replica) wing root fairings, in 2001-2002.

For info on these dies see the TM Tech website, http://www.tinmantech.com/products/f...-hammers/dies/
-- hopefully they are up now. If not, then we have to wait a bit ...
__________________
Kent

http://www.tinmantech.com

"All it takes is a little practical experience to blow the he!! out of a perfectly good theory." --- Lloyd Rosenquist, charter member AWS, 1919.

Last edited by crystallographic; 06-10-2017 at 03:54 PM.
Reply With Quote
  #2  
Old 06-10-2017, 05:42 PM
Dave K. Dave K. is offline
MetalShaper of the Month June 2017
 
Join Date: Oct 2016
Location: Orlando, Florida
Posts: 152
Default

Kent, I have watched your videos on this process and always amazed at the products. That lamp is cool!
__________________
Dave
Reply With Quote
  #3  
Old 06-11-2017, 05:23 AM
Gojeep's Avatar
Gojeep Gojeep is offline
MetalShaper of the Month March 2015, March 2020,, June 2022,Aug 2023
 
Join Date: Nov 2013
Location: Eastern Melbourne, Australia
Posts: 2,986
Default

Great information yet again.
__________________
Marcus
aka. Gojeep
Victoria, Australia
http://willyshotrod.com

Invention is a combination of brains and materials.
The more brains you use, the less materials you need.
Reply With Quote
  #4  
Old 06-12-2017, 06:13 PM
RockHillWill RockHillWill is offline
MetalShaper of the Month Jan 2019
 
Join Date: Oct 2009
Posts: 3,089
Default

Very creative and ingenious items. I am especially fond of the texturing dies. Do these items fit only your power hammers? We were using it this week on the steel inner fender wells for Jim's Bugatti project. I will look at his die selection the next time I visit and see what he has or needs.

How would these items be for 'finishing' the .060" #3003 aluminum panels?

I also added my name to the 'technical' report list found on your website.

Thanks for sharing.
__________________
Will
Reply With Quote
  #5  
Old 06-13-2017, 12:00 PM
crystallographic crystallographic is offline
MetalShaper of the Month October '14 , April '16, July 2020, Jan 2023
 
Join Date: Dec 2010
Location: Western Sierra Nevadas, Badger Hill, CA
Posts: 4,388
Default

Thank you, Dave, Marcus, and Will.

Will, I do not know what other hammering machines my tooling will work on. I know that one fellow who cloned the big CP planishers many years ago was copying my stuff but could not get it to work in his machines - when he finally called me I told him that planishers do not have the power to perform shaping operations.

I think I have some very good planishing tools for your .063 3003.

"The rising tide lifts all boats."
__________________
Kent

http://www.tinmantech.com

"All it takes is a little practical experience to blow the he!! out of a perfectly good theory." --- Lloyd Rosenquist, charter member AWS, 1919.
Reply With Quote
  #6  
Old 06-13-2017, 02:11 PM
RockHillWill RockHillWill is offline
MetalShaper of the Month Jan 2019
 
Join Date: Oct 2009
Posts: 3,089
Default

I, for one, am most appreciative of your willingness to add water regardless of hull design.
__________________
Will
Reply With Quote
Reply

Thread Tools Search this Thread
Search this Thread:

Advanced Search
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump

All times are GMT -5. The time now is 11:53 AM.

Powered by vBulletin® Version 3.8.11
Copyright ©2000 - 2024, vBulletin Solutions Inc.